Superalloys Heat-Resisting Alloys Based on Nickel 713c, M246

Model NO.: 713C(2.4671), 713LC, M246, GMR235, U500
Origin: China
Superalloys are indispensable materials in aviation navigation, military industry and so on. The master superalloys smelted by Vacuum induction furnace is one of our main products and its quality has reached advanced level at home and abroad, which can be used for making turbine vanes, guide vanes and other heat resistant components in aviation and other industries. Wrought Superalloys wire,strip,and bar can also be produesed.

 Mechanical Properties
Condition Tensile Property Stress Rupure Property
Cast Temperature
ºC
Rm
N/mm2
Rp0.2
N/mm2
A
%
Temperature
ºC
Stress
N/mm2
A
%
Life
hr
760±3 >860 >690 >4 871±2 414 >4 >24
Room
Temperature
>780 >680 >2 ---
 
Superalloys Heat-Resisting Alloys Based on Nickel 713c, M246


 

Outdoor Floor Tile

Outdoor floor tile combine the design of public and private spaces with sustainability, performance and flexibility. The outdoor porcelain tile main dimensions of the square brick are 108x108mm, 150x150mm, 200x200mm, 300x300mm, 400x400mm, 600x1200mm...


Applications: courtyard balconies, leisure plazas, municipal works, landscaping, school hospitals, and other home patio areas or public places with a large number of people.


Features:

1. The stone tile outdoor have passed the strict selection criteria and the unique high-temperature slow-burning technology, requiring a water absorption rate of <5%.

2. Good wear resistance, high flexural strength and excellent overall physical properties.

3. The outdoor non slip tile series is rich in variety, natural in texture and simple in texture. Through flexible and ingenious design of different specifications and various colors, it can collage colorful and different patterns, which can meet the outdoor space construction standards and decoration needs.


Construction attention point

1. Test the floor on the ground before paving, and distinguish the tile with different color numbers and sizes according to the paving form.

2. Side paving, side seaming, solid base layer and full joints can make the floor tile outside more durable and avoid rupture during use.

3. Tap the tile surface after paving to balance the tile bottom with the paving surface to avoid the phenomenon of empty drums.

4. Use the level gauge during the paving process to ensure the level of ceramic tile outdoor paving.

5. During the construction process, the cement or other sticky materials left on the tile surface should be wiped clean to avoid too long surface contamination and difficult to clean.

Stone Tile Outdoor,Outdoor Non Slip Tile,Outdoor Porcelain Tile,Ceramic Tile Outdoor,Floor Tile Outside

UMS New Materials Industry Co.,LTD , https://www.ums-factory.com